TY - GEN
T1 - Plasma co-polymerization technology with molecular-level structure tightening in "in-situ" SiOCH stacks for 32nm-node Cu interconnects
AU - Tada, M.
AU - Yamamoto, H.
AU - Ito, F.
AU - Narihiro, M.
AU - Ueki, M.
AU - Inoue, N.
AU - Abe, M.
AU - Saito, S.
AU - Takeuchi, T.
AU - Furutake, N.
AU - Onodera, T.
AU - Kawahara, J.
AU - Arai, K.
AU - Kasama, Y.
AU - Taiji, T.
AU - Tohara, M.
AU - Sekine, M.
AU - Hayashi, Y.
PY - 2006
Y1 - 2006
N2 - A novel plasma co-polymerization technology, using flexibly-mixed molecular gas of chain-type vinyl-siloxane and 6-membered ring-type one, has been developed for new Seamless Low-k SiOCH Stacks (SEALS). An ultimate high-modulus silica-amorphous-carbon-composite (SACC)-SiOCH film with 24.8GPa was realized by 100%-injection of the chain-type siloxane, adapting to the hard-mask on molecular-pore-stack (MPS) SiOCH film (k=2.45, 3.0GPa) from 100%-injection of the ring-type siloxane. For the via-dielectrics was utilized a new co-polymerized (CP) SiOCH film (k=2.8, 12.6GPa) from these gas mixture to enhance the mechanical strength. The in-situ sequential deposition of three kinds of films without air-break accomplished excellent adhesion, high quality interface and low O2 ashing damage. The fully-scaled-down, 32nm-node Cu interconnects achieved 83fF/mm (single-load) in 100nm-pitched Cu lines with the new co-polymerized SEALS.
AB - A novel plasma co-polymerization technology, using flexibly-mixed molecular gas of chain-type vinyl-siloxane and 6-membered ring-type one, has been developed for new Seamless Low-k SiOCH Stacks (SEALS). An ultimate high-modulus silica-amorphous-carbon-composite (SACC)-SiOCH film with 24.8GPa was realized by 100%-injection of the chain-type siloxane, adapting to the hard-mask on molecular-pore-stack (MPS) SiOCH film (k=2.45, 3.0GPa) from 100%-injection of the ring-type siloxane. For the via-dielectrics was utilized a new co-polymerized (CP) SiOCH film (k=2.8, 12.6GPa) from these gas mixture to enhance the mechanical strength. The in-situ sequential deposition of three kinds of films without air-break accomplished excellent adhesion, high quality interface and low O2 ashing damage. The fully-scaled-down, 32nm-node Cu interconnects achieved 83fF/mm (single-load) in 100nm-pitched Cu lines with the new co-polymerized SEALS.
UR - https://www.scopus.com/pages/publications/46049099839
UR - https://www.scopus.com/pages/publications/46049099839#tab=citedBy
U2 - 10.1109/IEDM.2006.346781
DO - 10.1109/IEDM.2006.346781
M3 - Conference contribution
AN - SCOPUS:46049099839
SN - 1424404398
SN - 9781424404391
T3 - Technical Digest - International Electron Devices Meeting, IEDM
BT - 2006 International Electron Devices Meeting Technical Digest, IEDM
T2 - 2006 International Electron Devices Meeting, IEDM
Y2 - 10 December 2006 through 13 December 2006
ER -