Failure assessment diagram analysis of high density polyethylene pipes

Jae Jun Han, Ho Wan Ryu, Yun Jae Kim, Jong Sung Kim, Young Jin Oh, Heung Bae Park

研究成果: Article査読

12 被引用数 (Scopus)

抄録

This paper presents an analysis of failure assessment diagram for PE4710 grade high density polyethylene pipes, which are recently concerned to use in the nuclear industry. Available test data of tensile, single edge notched tension specimens and pressurised pipes are summarised and suitably characterised for use in the failure assessment diagram in R6 procedure. Critical crack lengths and failure mode for the pressurised pipes and single edge notched tension specimens are determined under sustained load and compared with test results. Based on the concept of linear elastic fracture mechanics, a slow crack growth rate of PE4710 at 95°C is obtained excluding crack initiation time. To consider the effect of temperature on slow crack growth rate, a shift method is introduced. Remaining life is calculated against the crack margin and compared with the failure time.

本文言語English
ページ(範囲)4929-4938
ページ数10
ジャーナルJournal of Mechanical Science and Technology
28
12
DOI
出版ステータスPublished - 2014 12月
外部発表はい

ASJC Scopus subject areas

  • 材料力学
  • 機械工学

フィンガープリント

「Failure assessment diagram analysis of high density polyethylene pipes」の研究トピックを掘り下げます。これらがまとまってユニークなフィンガープリントを構成します。

引用スタイル