Hydrogen-assisted stress corrosion cracking simulation using the stress-modified fracture strain model

  • Nak Hyun Kim
  • , Chang Sik Oh
  • , Yun Jae Kim
  • , Kee Bong Yoon
  • , Young Wha Ma

研究成果: Article › 査読

23   !!Link opens in a new tab 被引用数 (Scopus)

抄録

This paper proposes a numerical method to simulate hydrogen-assisted stress corrosion cracking, via coupled diffusion elastic-plastic finite element damage analyses based on phenomenological stress-modified fracture strain model. For validation, simulated results using the proposed method are compared with published experimental data of FeE 690T compact tension tests under air and hydrogen condition with various constant load-line displacement rates. The simulated results agree well with experimental data.

本文言語English
ページ(範囲)2631-2638
ページ数8
ジャーナルJournal of Mechanical Science and Technology
巻26
号8
DOI
出版ステータスPublished - 2012 8月
外部発表はい

ASJC Scopus subject areas

  • 材料力学
  • 機械工学

フィンガープリント

「Hydrogen-assisted stress corrosion cracking simulation using the stress-modified fracture strain model」の研究トピックを掘り下げます。これらがまとまってユニークなフィンガープリントを構成します。

引用スタイル