抄録
The zero-field-cooled magnetization at the magnetic field H = 300 Oe shows anomolous kinks at TA and TB (> TA) far below the reentrant spin-glass-like transition temperature Tf (above which a long-range ferrimagnetic ordering is set up). The irreversibility between the zero-field-cooled and the field-cooled magnetizations, and the time decay of the thermoremanent magnetization (σTRM) are observed below the ferrimagnetic Curie temperature Tc. The decay feature can be described by Ogielski's power law σTRM = At-α whose α exhibits peaks at TA, TB, Tf and TC. The peak of α at TC can be fitted by the combination of Ising type and Ginzburg-Landan type expressions. Three stepwise changes of the spin-glass-like state below Tf and the feature of the coexistence of short-range spin-glass and long-range magnetic ordering components above Tf are discussed.
| 本文言語 | English |
|---|---|
| ページ(範囲) | 213-220 |
| ページ数 | 8 |
| ジャーナル | Physica Status Solidi (B) Basic Research |
| 巻 | 203 |
| 号 | 1 |
| DOI | |
| 出版ステータス | Published - 1997 9月 |
ASJC Scopus subject areas
- 電子材料、光学材料、および磁性材料
- 凝縮系物理学
フィンガープリント
「Long-time decay of thermoremanent magnetization through stepwise changes of the reentrant spin-glass-like state in the Ni2In-type Mn7Sn4」の研究トピックを掘り下げます。これらがまとまってユニークなフィンガープリントを構成します。引用スタイル
- APA
- Standard
- Harvard
- Vancouver
- Author
- BIBTEX
- RIS